Compliance Standards
ASTM C512
Technical parameters
- Maximum Testing Force : 500KN
- Measurement Range : 0-500KN
- Relative reading error : ±1%
- Spring Height : 300mm
- Spring Compression Stroke : 52mm (Or according to customerās requirement)
- Distance Between Upper Platen and Lower Platen (Compression space) : 1500mm (Or according to customerās requirement)
The equipment consists of following Parts :
- Main frame suitable for 3 Pieces of D150 x H300 mm concrete cylindrical samples
- Hand hydraulic pump (can replace with electric pump system at extra cost)
- Hydraulic jack
- Spoke sensor
- Ball plate (With harden treatment) connecting between sensor and sample